Welding seam defecting aerosol CRACK1 400ml

12.51

1. Clean the weld with a wire brush, then clean the surface with the cleaning aerosol Infinity Cleaner.

Spray the cleaner on the weld, wait approx. 30 seconds and wipe the surface dry with a cloth or paper towel.

2. Spray red penetrant WS1820S CRACK1 on the surface.

Wait 3-5 minutes. If the temperature is lower than 12 degrees, the time must be longer, if higher than 45 degrees, then shorter.

Clean the surface with a penetrant cloth or paper cloth, the cloth can be gently moistened.

3. Revealed (white) WS1821S CRACK2 spray on surface. It is recommended to spray 2-3 thin layers, the surface must remain slightly moist.

If too thick a layer is applied, the penetrant can cover the developer and the cracks will not be visible. You have to wait up to 5 minutes.

Red lines indicate cracks, red dots indicate fine cracks, and dots indicate pores.

Product code: prv_WS1820S Categories: ,

Description

Welding seam defecting aerosol CRACK1 400ml

Product description

Welding seam defecting aerosol CRACK1 400ml is specially designed for welding seam defects and error detection. This aerosol helps to detect cracks, pores and other defects in welds.

Manual

Step 1: Cleaning the weld

Before using the aerosol, the weld must be cleaned with a wire brush. The surface must then be cleaned with the cleaning aerosol Infinity Cleaner. Spray the cleaner on the weld, wait about 30 seconds and wipe the surface dry with a cloth or paper.

Step 2: Spraying the red penetrant

Spray the red penetrant on the surface of the WS1820S CRACK1. Wait 3-5 minutes. If the temperature is lower than 12 degrees, the waiting time must be longer, if the temperature is higher than 45 degrees, then shorter. Clean the surface of the penetrant with a cloth or paper, the cloth may be slightly moistened.

Step 3: Spray revealed

Spray the developer (white) on the surface of WS1821S CRACK2. It is recommended to spray 2-3 thin layers, the surface must remain slightly moist. If too thick a layer is applied, the penetrant can cover the developer and the cracks will not be visible. Wait until